COTTON (Fine 2 hrs)

$120.00

Material & Process:

2 pounds of Cotton Linter is Beat to a Pulp for 2 hours using a Reina brand Hollander beater. Water is partially strained, so that the Cotton Linter can be condensed into a plastic 5-gallon bucket for delivery, pickup and/or shipping.

Pulp Use:

Scoop the Cotton (Fine) Pulp from buckets into desired container and mix with Water. Cotton (Fine) are fine, short, small, smooth fibers beat to run through: syringe, dropper, squeeze bottle or spray bottle. This Type Beat is best for Pulp Imaging, Pulp Painting and Pigment Layering. Mix Cotton (Fine) with Pigment, Retention Aid and Water for consistent color.

Internal Sizing:

We add 1 tbsp of sizing per pound of fiber. Sizing is added to the pulp during the last 10 minutes of beating. Internal Sizing reduces the potential for absorbency, lessening the potential for bleeding of inks, paints or pigments. Sizing protects the fiber from oils, dirt and debris. Chicago Pulp uses Alkylketene Dimer liquid sizing concentrate.

PULP COTTON (Fine 2 hrs)
Quantity:
Add To Cart

Material & Process:

2 pounds of Cotton Linter is Beat to a Pulp for 2 hours using a Reina brand Hollander beater. Water is partially strained, so that the Cotton Linter can be condensed into a plastic 5-gallon bucket for delivery, pickup and/or shipping.

Pulp Use:

Scoop the Cotton (Fine) Pulp from buckets into desired container and mix with Water. Cotton (Fine) are fine, short, small, smooth fibers beat to run through: syringe, dropper, squeeze bottle or spray bottle. This Type Beat is best for Pulp Imaging, Pulp Painting and Pigment Layering. Mix Cotton (Fine) with Pigment, Retention Aid and Water for consistent color.

Internal Sizing:

We add 1 tbsp of sizing per pound of fiber. Sizing is added to the pulp during the last 10 minutes of beating. Internal Sizing reduces the potential for absorbency, lessening the potential for bleeding of inks, paints or pigments. Sizing protects the fiber from oils, dirt and debris. Chicago Pulp uses Alkylketene Dimer liquid sizing concentrate.

PULP COTTON (Fine 2 hrs)

sign up for our newsletter to receive updates about Pulp, Process, Practice and More.

Thank you! Your response has been recorded. Welcome to the Chicago Pulp Newsletter!

Sincerely,

the Chicago Pulp Team!

Contact: info@chicagopulp.com

CHICAGO PULP NEWSLETTER

chicago pulp

1100 West 37th Street Suite #002

Chicago Illinois, 60609


info@chicagopulp.com
By appointment only.